Appearance: Light Yellow To Brown Liquid
Acid Value: (mg KOH/g) 2-40
Amine Value: (mg KOH/g) 2-40
Density: 0.80-1.00g/cm3
Viscosity Cps: (25℃) 100-1000
Active Ingredient: 50%
Solvent: White Mineral Oil
Basic Infomation
Place of Origin: China
Brand Name: Anjeka
Certification: ISO9001-2015
Model Number: Anjeka6042A
Payment & Shipping Terms
Packaging Details: 25kg/drum
Delivery Time: 3-5days
Payment Terms: L/C, D/P, T/T, Western Union
Supply Ability: 100tons/month
Product Description

ANJEKA-6042A

 

GENERAL DESCRIPTION

Polymer dispersants for dispersing colorants in low polarity ceramic inkjet inks.

 

PRODUCT DATA

Chemical composition: Highly branched polymer solution.

Typical Physical and Chemical Data:

The data given on this data sheet are typical values and are not product specifications.

Appearance: Light yellow to brown liquid

Acid value (mg KOH/g) 2-40

Amine value (mg KOH/g) 2-40

Density g/cm³ (23℃) 0.80-1.00

Viscosity cps (25℃) 100-1000

Active ingredient (%) 50

Solvent White mineral oil

 

STORAGE and TRANSPORT

Please stir well before use, delamination or turbidity may occur when the temperature is lower than 0℃, it should be heated to 30℃-40℃ and stirred well before use.

 

APPLICATION GUIDELINES

Ceramic Ink Features and Benefits

Anjeka-6402A can be used in low polarity ceramic inkjet inks with hydrocarbon and fatty acid esters, either as a dispersant alone or in combination with other products. This product also helps to shorten the grinding time and filtration time of ceramic colorant slurry, improve productivity, and prepare ceramic inks with Newtonian fluid properties. It helps to improve the storage stability of the colorants in ceramic inks, reduce sedimentation, and improve the vivid color.

 

APPLICATION SECTORS

This additive is recommended for dispersing colorants in ceramic inks.

 

RECOMMENDED LEVELS

Dosage of additives (in purchased form) based on the pigment: 10%-50%.

The optimum dosage should be determined through a series of tests.

 

INCORPORATION AND PROCESSING INSTRUCTIONS

For best performance, the additive should be added to the abrasive first, mixed well and then added to the colorant.

 

PACKAGING

-25kg iron drum with inner coating

-200kg ring plastic drum

 

Our service

 

1. Reply within 24 hours.
2. High-quality products and reasonable price
3.R&D technology support.
4. Professional team service
5. Customiszed production for different package
6. No delay on shipment

 

polymer disperant ANJEKA 6042A low polarity ceramic inkjet ink BYK P4100 0

 

Recommended Products
Get in touch with us
Contact Person : Ms. Anna
Tel : +8615171019131
Fax : 86-0711-3809626
Characters Remaining(20/3000)