GENERAL DESCRIPTION
ANJEKA-6062B
GENERAL DESCRIPTION
Anjeka-6062B is suitable for solvent-based and solvent-free systems, offering
excellent dispersion performance and broad compatibility with various systems. It is
highly recommended for universal pigment concentrate dispersion applications.
PRODUCT INFORMATION
Chemical Composition: Solution of a high-molecular-weight polymer containing
pigment-affinic functional groups.
Typical Physicochemical Data:
The data provided on this sheet are typical values and not product specifications.
Appearance: Yellow transparent liquid
Acid Value (mg KOH/g): 1–10
Amine Value (mg KOH/g): 1–10
Density (g/cm³ at 23°C): 1.00–1.20
Viscosity (cps at 25°C): 25–300
Active Content (%): 40
Solvent: Ethylene glycol diacetate
STORAGE AND TRANSPORT
Store in a cool, dry place. Mix thoroughly before use. Separation or cloudiness may
occur below 0°C; warm to 20°C and mix well.
Storage duration is not recommended to exceed 12 months.
APPLICATION
Industrial Coatings
Features and Benefits:
This additive achieves pigment deflocculation through steric hindrance. The
deflocculated pigments exhibit fine particle sizes, resulting in high gloss, enhanced
color strength, improved transparency for transparent pigments, and increased opacity
for opaque pigments. It also reduces viscosity, improves flow properties, and allows
higher pigment loading in color concentrates.
APPLICATION SECTORS
Anjeka-6062B demonstrates good compatibility with alkyd resins, cellulose,
chlorinated rubber, epoxy, polyurethane, polyester, and acrylates.
Industrial Coatings ●
Automotive Coatings ●
Architectural Coatings ○
Printing Inks ○
(●—Specially recommended; ○—Recommended)
RECOMMENDED LEVELS
The following additions are based on the ratio of dispersant solids to pigment weight:
Inorganic pigments: 5%–10%
Titanium dioxide: 1%–3%
Organic pigments: 10%–35%
Carbon black: 15%–75%
These are empirical values; optimal dosage should be determined through testing.
INCORPORATION AND PROCESSING INSTRUCTIONS
For optimal performance, add during the grinding stage before introducing pigments.
PACKING
25 kg inner-coated iron drum
180 kg plastic drum